Ceramic Welding Repair

Ceramic welding repair
Glass furnaces parapet walls of molten pool, little furnace, hook turn and big top self-closed, regenerative chamber partition, small stove legs, self-closed areas such as the Angle of the breakage of the ordinary maintenance, hot fix method can not use ceramic weld repairs can get good maintenance effect.

(1) The molten pool parapets -- before, during and after weld repairs


(2) The molten pool hook - before, during and after weld repairs

 

(3) Qian the self-closed ping - before, during and after weld repairs


(4) Small stove legs - before, during and after weld repairs


(5) The self-closed top - before, during and after weld repairs

(6) Crater flat self-closed - before, during and after weld repairs


(7) Before the face of wall - before, during and after weld repairs


(8) L hanging wall - before, during and after weld repairs

(9) Air chamber wall, before, during and after weld repairs

(10) The gas chamber partition - before and after weld repairs

(11) Small furnace flat self-closed - before and after weld repairs


(12) Ceramic after weld repairs to cold repair

(13) after welding repair to cold repair


The pool arch top welding after 2 years


The pool arch bricks 3M2 welding after 2 years


1 years after the pool arch angle welding

Small furnace neck welding repair 2 years later


           leg welding repair 30 months later

2 years after wall welding in regenerator room